The proprietary K-LEAN™ surface is created by two sequential stages: sandblasting, aimed at creating a porous surface topography, followed by acid etching, intended to generate micro-roughened surface structure. The surface treatment is completed by removing contaminants using ultra-pure water (UPW), a unique process acquired from the semiconductor industry.1,2,3